Harris Euro Welding Alloys

Product Description
MODEL ALLOY % FEATURE
Ag Cu P Sn Zn
Silver Virgin Phosphorus Tin Zinc
L – CuP6
(Square)
93.7 6.3 Application Area : Copper-Copper Resources
Fluidity : Middle
Melting Boiling Range : 840 °C – 710 °C
L – CuP7
(Round)
92.8 7.2 Application Area : Copper-Copper Resources
Fluidity : Middle
Melting Boiling Range : 840 °C – 710 °C
HARRIS 0
(Flat)
93.2 6.8 Application Area : Copper-Copper Resources
Fluidity : High
Melting Boiling Range : 802 °C – 710 °C
L – Ag2p 2 84.7 6.3 7 Application Area : Bakır-Bakır Kaynaklarında
Fluidity : High
Melting Boiling Range : 824 °C – 643 °C
DYNAFLOW 6 87.9 6.1 Application Area : Copper-Copper Resources
Fluidity : Middle
Melting Boiling Range : 798 °C – 643 °C
L – Ag18P 18 75 7 Application Area : Bakır-Bakır Kaynaklarında
Fluidity : High
Melting Boiling Range : 779 °C – 643 °C
L – AG20 FC
Borax Coated
20 45 35 Application Area : Copper-Copper, Copper-Iron Sources
Fluidity : High
Melting Boiling Range : 810 °C – 690 °C
L – Ag30 30 38 32 Application Area : Copper-Copper, Copper-Iron Sources
Fluidity : High
Melting Boiling Range : 795 °C – 690 °C
L-Ag40 SnFC
Borax Coated
40 30 2 28 Application Area : Copper-Copper, Copper-Iron Sources
Fluidity : High
Melting Boiling Range : 700 °C – 640 °C